FIELD: chemistry.
SUBSTANCE: glaze comprises, wt %: SiO2 59.0-61.0; Al2O3 9.0-11.0; MgO 12.0-13.0; CuO 1.0-1.5; K2O 1.8-3.0; ZrO2 2.0-3.0; 3Al2O3⋅2SiO2 10.0-13.0.
EFFECT: increase in the thermal stability of glaze.