FIELD: chemistry.
SUBSTANCE: method of leaching the wastes of enriched amorphous magnesite with a solution of nitric acid is described, in which serpentinite-magnesite screening of fraction of 2 mm was ground in a vibratory mill for 0.5 h, the resulting powder in an amount of 10 kg was loaded through a metering hopper into the leaching reactor, where after addition of 40% of the solution of nitric acid in the ratio of 1/3 g/ml, mixing with ultrasound and heating to 90°C are carried out, the leaching reaction of serpentinite was carried out for 2 hours.
EFFECT: increasing the leaching efficiency.
1 dwg,1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING HEXAHYDRATE OF MAGNESIUM NITRATE THROUGH COMPLEX PROCESSING SERPENTINITE | 2008 |
|
RU2395457C1 |
METHOD OF OBTAINING MAGNESIUM OXIDE | 2012 |
|
RU2513652C2 |
METHOD OF PROCESSING OF SERPENTINITE | 2005 |
|
RU2292300C1 |
METHOD OF PRODUCING MAGNESIUM SULPHATE FROM MAGNESIUM-CONTAINING RAW MATERIAL | 2019 |
|
RU2727382C1 |
METHOD FOR PROCESSING OF OXIDISED NICKEL ORES | 2013 |
|
RU2532871C1 |
METHOD OF PREPARING MAGNESIUM HYDROXIDE | 1993 |
|
RU2069176C1 |
METHOD OF PRODUCING FINELY DISPERSED SILICON DIOXIDE | 2015 |
|
RU2593861C1 |
METHOD OF OBTAINING MAGNESIUM OXIDE | 2012 |
|
RU2535690C2 |
METHOD OF COMPLEX REPROCESSING OF MAGNESIUM-SILICATE RAW MATERIALS | 2005 |
|
RU2285666C1 |
METHOD FOR PROCESSING SYNNYRITE | 2020 |
|
RU2753109C1 |
Authors
Dates
2018-01-25—Published
2016-12-22—Filed