FIELD: chemistry.
SUBSTANCE: composition for manufacturing heat-sensitive paper contains a fibrous mixture of 60-80 wt % of cellulose and 20-40 wt % of a chemical-thermomechanical mass obtained by grinding the hardwood chips in two stages. Chemical processing of wood chips before the first stage of grinding is carried out in the presence of deresinator containing anionic, nonionic, cationic, and amphoteric surfactants and isopropyl alcohol with 0.10-0.15 wt % of the absolutely dry wood chips. Before the second stage of grinding, a chemical treatment is carried out in the presence of a deresinator containing anionic, nonionic, and amphoteric surfactants, as well as salts from the group consisting of phosphates, carbonates, silicates, and chelates at a rate of 0.05-0.09% of the absolutely dry wood chips.
EFFECT: replacement of a part of expensive cellulose with a modified bleached chemico-thermomechanical mass from hardwood is provided without loss of mechanical strength of paper.
2 cl, 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD TO PRODUCE CELLULOSE FOR SANITARY-HYGIENE TYPES OF PAPER | 2011 |
|
RU2488653C2 |
METHOD OF PRODUCING CELLULOSE FOR CHEMICAL PROCESSING | 2020 |
|
RU2738813C1 |
METHOD OF PREPARING BLEACHED CHEMICO-THERMOMECHANICAL PULP | 1999 |
|
RU2153545C1 |
COMPOSITION TO MAKE CHALK OVERLAY PAPER | 2010 |
|
RU2434091C1 |
METHOD OF PREPARATION OF CELLULOSE FOR NITRATION | 2017 |
|
RU2674198C1 |
CHEMICAL-THERMOMECHANICAL MASS PREPARATION PROCESS | 2005 |
|
RU2287034C1 |
METHOD OF PREPARING WHITENED CHEMICAL-THERMOMECHANICAL MASS FROM LARCH WOOD | 1995 |
|
RU2074919C1 |
PAPER PULP FOR MANUFACTURE OF DAILY PAPER | 1995 |
|
RU2085645C1 |
CELLULOSE-COMPOSITE MATERIAL | 2023 |
|
RU2802036C1 |
PULP FOR MAKING BACKING PAPER FOR PLYWOOD LINING | 0 |
|
SU1756442A1 |
Authors
Dates
2018-01-26—Published
2016-12-16—Filed