FIELD: technological processes.
SUBSTANCE: invention can be used in the polymeric materials production: paint and varnish coatings, plastics, compounds, sealants, adhesives, rubbers. White pigment particles agglomerates production process comprises the mineral filler pre-calcination and subsequent filler particles and titanium dioxide joint grinding. As the mineral filler, mixture of kaolin and hydrated alumina is used with the following wt. ratio: kaolin 50–80, hydrated alumina 20–50. Filler content makes up to 40 parts by weight per 100 parts by weight of the pigment. Calcination is carried out at a temperature of 450–500 °C for 2–3 hours. Joint grinding is carried out at a temperature of 100–150 °C.
EFFECT: invention allows to partly replace the titanium dioxide in the white pigment composition with more affordable and inexpensive materials without significant loss in the pigment whiteness and covering quality.
3 cl, 1 tbl, 11 ex
Title | Year | Author | Number |
---|---|---|---|
WHITE PIGMENT | 2015 |
|
RU2607221C1 |
WHITE PIGMENT | 2015 |
|
RU2607406C1 |
WHITE PIGMENT | 2015 |
|
RU2613052C1 |
WHITE PIGMENT | 2015 |
|
RU2613055C2 |
METHOD OF PREPARING ATMOSPHERE-RESISTANT PIGMENT FROM TITANITE CONCENTRATE | 2002 |
|
RU2236426C2 |
METHOD OF SPHENE CONCENTRATE PROCESSING | 1996 |
|
RU2096331C1 |
METHOD OF OBTAINING TITANIFEROUS PRODUCT FROM SPHENE CONCENTRATE | 2007 |
|
RU2356837C1 |
ACRYLIC PAINT SYSTEM | 2008 |
|
RU2357991C1 |
SILICATE PAINT | 2013 |
|
RU2540434C1 |
PROCESS FOR PRODUCING TITANIUM DIOXIDE PIGMENT | 0 |
|
SU1074883A1 |
Authors
Dates
2018-08-30—Published
2017-06-20—Filed