FIELD: construction.
SUBSTANCE: invention relates to construction materials and can be used in civil, industrial, road and special construction. Heat-insulating structural concrete made from concrete mixture, consists of portland cement PC700-B (CEM 1.62.5 B), microspheres of 0–500 mcm fraction, microspheres of 0–50 mcm fraction, polycarboxylate hyperplasticizer "Melflux 2651F", crushed-ash slag screenings of 0–10 mcm fraction, fiber with diameter of 10 mcm and length 500 mcm, with the following ratio of components, wt%: Portland cement PC700-B (CEM 1.62.5 B) – 18…21, microspheres 0–500 mcm – 50…58, microspheres 0–50 mcm – 5…12, hyperplasticizer 0.15…0.2, crushed-stone ash-slag screenings of 0–10 mcm fraction – 1.5…1.7, basalt fiber glass 10×500 mcm – 0.8…0.85, water – balance.
EFFECT: obtaining concrete with coefficient of heat conductivity λ≤0,14 W/m*K and compression strength Rcomp≥12,5 MPa.
1 cl, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
HIGH-STRENGTH LIGHT CONCRETE | 2012 |
|
RU2515450C1 |
LIGHTWEIGHT CONCRETE FOR STRUCTURAL, HEAT-INSULATING AND STRUCTURAL PURPOSES | 2022 |
|
RU2783073C1 |
HIGH-STRENGTH LIGHT FIBROUS CONCRETE | 2014 |
|
RU2548303C1 |
LIGHTWEIGHT CONSTRUCTION COMPOSITE | 2021 |
|
RU2773899C1 |
NANOMODIFIED HIGH-STRENGTH LIGHT CONCRETE | 2019 |
|
RU2718443C1 |
FINE-GRAINED SELF-COMPACTING CONCRETE MIX | 2022 |
|
RU2778123C1 |
MIXTURE FOR MAKING CEMENT-CONTAINING CONSTRUCTION MATERIAL | 2017 |
|
RU2708138C1 |
SELF-COMPACTING CONCRETE MIXTURE | 2016 |
|
RU2632795C1 |
HIGH-STRENGTH POWDER-ACTIVATED CONCRETE | 2020 |
|
RU2738150C1 |
NANO-MODIFYING HIGH-STRENGTH LIGHTWEIGHT CONCRETE BASED ON COMPOSITE BINDER | 2021 |
|
RU2775585C1 |
Authors
Dates
2019-09-24—Published
2018-10-24—Filed