FIELD: metallurgy.
SUBSTANCE: inventions can be used in producing a welded joint containing FeCrAl and FeNiCr alloys. During welding, filler metal is used, containing ingredients in specified ratio. Connectable parts can be made in the form of pipes and/or strips. Welding metal made in form of wire or strip is used.
EFFECT: parts containing said weld joint can be operated at temperature equal to or greater than 650 °C.
12 cl, 4 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
NICKEL-BASED ALLOY TO FORM ALUMINIUM OXIDE | 2009 |
|
RU2518812C2 |
PIPE AND PIPE MANUFACTURING METHOD | 2016 |
|
RU2732395C2 |
WELDING WIRE FOR Fe-36Ni ALLOY | 2013 |
|
RU2629122C2 |
HIGH-TEMPERATURE ALLOY | 2015 |
|
RU2580765C1 |
METHOD OF MAKING PIPE DEVICE, PIPE DEVICE AND OVEN EQUIPPED WITH SUCH PIPE DEVICE | 2016 |
|
RU2711168C2 |
HIGH-TEMPERATURE ALLOY | 2015 |
|
RU2581323C1 |
HIGH-TEMPERATURE ALLOY | 2015 |
|
RU2581317C1 |
HIGH-TEMPERATURE ALLOY | 2015 |
|
RU2579405C1 |
METHOD FOR PRODUCTION OF WELDED STEEL BILLET AND CORRESPONDING WELDED STEEL BILLET | 2019 |
|
RU2783829C1 |
HIGH-TEMPERATURE ALLOY | 2015 |
|
RU2581322C1 |
Authors
Dates
2020-03-16—Published
2016-06-30—Filed