FIELD: pressure processing of metals.
SUBSTANCE: invention can be used in manufacturing of piercer plug. At the first transition, the original blank is upset to form the input cone of the blank. At the second transition, by direct extrusion, a conical blank is obtained without an end protrusion with a height equal to 0.75-0.90 of the height of the finished plug. The maximum cone diameter in the upper part is equal to 0.95-0.98 of the plug diameter, in the lower part - 1.0-1.3 of the plug diameter adjacent to the end shoulder of the plug. In the middle part, the diameter is 0.7-0.9 of the diameter of the finished plug in the corresponding section. At the third transition, the combined extrusion of the inner cavity of the plug and the end protrusion is performed, at the fourth transition - the final shaping by open stamping of the rear conical section of the plug.
EFFECT: reduction in technological effort, increase of durability of the piercing tool, and increase of the depth of the plug cavity.
4 cl, 5 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING WATER-COOLED PIERCING MILL MANDREL IN FORM OF TWO-LAYER HOLLOW BODY AND STAMP FOR ITS IMPLEMENTATION | 2023 |
|
RU2804236C1 |
METHOD FOR RESTORING OUTER SURFACE OF PIERCING MILL MANDRELS AND STAMP FOR ITS IMPLEMENTATION | 2023 |
|
RU2806565C1 |
WATER-COOLED MANDREL OF SKEW-ROLL PIERCING MILL, METHOD OF MAKING SAID MANDREL AND DIE TOOLING FOR MANUFACTURE THEREOF | 2023 |
|
RU2816967C1 |
METHOD OF PRODUCING MANDREL FOR BROACHING MILL | 0 |
|
SU904855A1 |
METHOD OF MANUFACTURING PIERCING MILL MANDRELS | 0 |
|
SU1129009A1 |
PUNCHING METHOD OF WELDING NECK FLANGE FORGING | 2007 |
|
RU2352431C2 |
METHOD FOR MANUFACTURING HOLLOW ARTICLES | 0 |
|
SU1807914A3 |
METHOD OF PRODUCING HOLLOW ARTICLES | 0 |
|
SU1480947A1 |
METHOD OF FORMING ROD PARTS HAVING HEAVY HEAD WITH CAVITY | 1991 |
|
RU2083312C1 |
METHOD OF PRODUCING CYLINDRICAL GEARS | 0 |
|
SU946781A1 |
Authors
Dates
2023-03-13—Published
2022-07-01—Filed