FIELD: refractory mixtures.
SUBSTANCE: invention relates to production of refractory mixture, which can be used as masonry mortar and for coating during lining and repair works of thermal units. Refractory mixture contains chromite ore, iron oxide, magnesium sulphate or aluminium sulphate, periclase, as well as aluminium or an alloy of aluminium and silicon, and additionally contains a silicate lump used as flux, in the following ratio, wt.%: chromite ore 44.0–66.4, iron oxide 10.0–21.0, aluminium or aluminium and silicon alloy 9.0–15.0, periclase 5.0–10.0, magnesium sulphate or aluminium sulphate 7.0–15.0, silicate lump 0.5–1.0.
EFFECT: obtained mixture composition enables to reduce ignition temperature to values of 710–750 °C and has refractoriness of 1,680–1,770 °C.
1 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY MIX | 1999 |
|
RU2138464C1 |
METHOD OF HOT RELINING OF COKE OVENS AND GAMMA-2KS THERMITE MASS FOR METHOD EMBODIMENT | 2001 |
|
RU2187484C1 |
MORTAR FOR LINING HIGH TEMPERATURE UNITS | 1992 |
|
RU2065426C1 |
HEAT-RESISTANT MASONRY MORTAR | 2009 |
|
RU2387622C1 |
METHOD OF COMPLEX PROCESSING OF SERPENTINE-CHROMITE CRUDE ORE | 2013 |
|
RU2535254C1 |
SAND MIX BACKING MATERIAL | 2010 |
|
RU2414321C1 |
CHARGE MATERIAL FOR PRODUCTION OF NONSHRINKING, POROUS, FLAMEPROOF HEAT INSULATING MATERIAL | 2010 |
|
RU2442761C1 |
METHOD OF INTEGRATED PROCESSING OF MAGNESIUM-CHROME CRUDE ORE | 2006 |
|
RU2344076C2 |
SLAG-FORMING MIXTURE FOR CONTINUOUS STEEL POURING | 2014 |
|
RU2555277C1 |
FIRE-RESISTANT MIX AND METHOD FOR TEMPERING THEREOF | 2002 |
|
RU2211200C1 |
Authors
Dates
2024-02-19—Published
2023-06-16—Filed