FIELD: switching devices. SUBSTANCE: one of the contacts of the contact pair is made of a silver-cadmium oxide compound (8 to 22 percent by mass), and the other - of an intermetallic compound (Ti 42 to 47.5; Fe 2.5 to 4.5 percent by mass); Ni - the rest. The contact pair features an erosion resistance increased by 38 to 42% at a high resistance to sticking. EFFECT: enhanced erosion resistance.
Title | Year | Author | Number |
---|---|---|---|
CONTACT PAIR | 0 |
|
SU1735927A1 |
WIRE OF SILVER-CONTAINING MATERIAL FOR PRODUCING ELECTRIC CONTACTS | 2002 |
|
RU2219608C1 |
CAKED SILVER BASED MATERIAL FOR ELECTRIC CONTACTS | 1984 |
|
SU1198969A1 |
SILVER BASED MATERIAL FOR ELECTRIC CONTACTS | 1984 |
|
SU1208821A1 |
MIXTURE FOR PROCESS PRECOAT OF CERMET ELECTRIC CONTACTS | 1985 |
|
SU1355024A1 |
LAMINATED ELECTRIC CONTACT | 1991 |
|
RU2033653C1 |
CHARGE PREPARING METHOD | 1988 |
|
SU1577173A1 |
SILVER-BASED ALLOY | 1986 |
|
SU1405339A1 |
METHOD OF PRODUCING COMPOSITE MATERIAL FOR COPPER-BASED ELECTRIC CONTACTS | 2009 |
|
RU2398656C1 |
MATERIAL FOR ELECTRIC CONTACTS BASED ON COMPOSITION OF SILVER-LEAD OXIDE | 1993 |
|
RU2032954C1 |
Authors
Dates
1994-04-15—Published
1986-04-24—Filed