FIELD: chemical technology, inorganic chemistry. SUBSTANCE: titanium tetrachloride is dissolved in distilled water up to the concentration (as TiO2) 130-160 g/l, ratio of free hydrochloric acid to titanium dioxide is made 1.4-1.8, and titanium (3+) chloride is added to the solution at concentration of TiO2 1-2 g/l. Solution is heated to 70-75 C and anatase modification seed charges were added to its at concentration 5-20 wt.-% with regard to TiO2 in the parental solution. Solution is heated at stirring up to 95-98 C and kept at this temperature at least 3-3.5 hr. Obtained hydrated TiO2 is filtered, washed with bidistilled water, dried and calcined at 600-650 C. Obtained TiO2 of anatase modification shows friable powder of monodispersed composition, particle size is 3-5 mcm, specific surface is the range 10-50 m2/g, basic substance content is 98-99%, impurity content - 1•10-5 wt.-%, not above. Calcination loss is 1-2%, not above. EFFECT: enhanced purity, particle size, decreased loss. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING TITANIUM DIOXIDE OF ANATASE MODIFICATION | 0 |
|
SU1546426A1 |
METHOD OF PRODUCING TITANIUM DIOXIDE OF ANATASE MODIFICATION | 0 |
|
SU1323535A1 |
PROCEDURE FOR PROCESSING TITANIUM-MAGNETITE CONCENTRATE | 2009 |
|
RU2394926C1 |
METHOD OF PRODUCING CRYSTALLINE TITANIUM DIOXIDE IN ANATASE STRUCTURAL MODIFICATION | 2014 |
|
RU2575026C1 |
METHOD OF PREPARING TITANIUM DIOXIDE | 1997 |
|
RU2130428C1 |
METHOD FOR PREPARATION OF MOLDED VANADIUM-TITANIUM CATALYST FOR CLEANING GASES | 1990 |
|
RU2050194C1 |
PROCESS FOR PRODUCING PIGMENT TITANIUM DIOXIDE OF ANATASE OF RUTILE MODIFICATION | 0 |
|
SU929670A1 |
METHOD OF PROCESSING OF LOPARITE CONCENTRATE | 2000 |
|
RU2182887C2 |
METHOD OF TITANIUM DIOXIDE PRODUCING (VARIANTS) | 1998 |
|
RU2142414C1 |
PROCESS FOR PRODUCING RUTILE TITANIUM DIOXIDE | 0 |
|
SU975578A1 |
Authors
Dates
1996-05-20—Published
1986-05-05—Filed