FIELD: deposition of metal coatings. SUBSTANCE: method involves subjecting metal article to vibrations of over 100 Hz and amplitude of 0.01-0.04 mm in the direction coinciding with that of plasma flow. Coating is applied in several layers of which the first ones are such metals as Cu, Ni, Cr and/or alloys thereof. Before plasma deposition, the surface of parts is roughened to 18-20 microns and heated to 160-180 C. EFFECT: higher efficiency. 2 cl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PLASMA SPRAYING OF COATS | 2004 |
|
RU2283364C2 |
PROCESS OF SURFACE PREPARATION FOR PLASMA COATING | 1998 |
|
RU2132402C1 |
METHOD OF COAT APPLICATION USING PULSE POWER ARC | 2011 |
|
RU2503739C2 |
PROCEDURE FOR APPLICATION OF PARTICLES ON THIN WALL METAL ITEM | 2009 |
|
RU2428501C2 |
APPLICATION METHOD OF THIN-FILM COATING ON METAL WORKS | 2007 |
|
RU2354743C2 |
METHOD OF FORMING COATINGS FROM SELF-FLUXING POWDERED MATERIALS ON IRON-CARBON ALLOY ARTICLES | 1997 |
|
RU2112815C1 |
METHOD FOR EVAPORATING FILM ON SUBSTRATE | 2000 |
|
RU2185006C1 |
METHOD OF MAKING EROSION-RESISTANT HEAT-PROTECTIVE COATS | 2003 |
|
RU2283363C2 |
METHOD OF MULTIFUNCTIONAL COATINGS PLASMA SPUTTERING | 2015 |
|
RU2604086C1 |
METHOD OF APPLYING CONTACT COATING ONTO THE CONTACT-PART OF VACUUM HIGH-VOLTAGE FERREED SWITCH | 0 |
|
SU1394258A1 |
Authors
Dates
1994-01-15—Published
1992-03-19—Filed