FIELD: metal industries. SUBSTANCE: crystallizer has copper working wall sides and channels provided with longitudinal ribs in their upper sections which run along the distance comprising from 0.1 to 0.3 of the wall side length. The ratio of the crystallizer upper and lower parts total channel working surface cross section perimeter is equal from 1.1 to 10.0. EFFECT: reduced copper consumption; increased effectiveness of ingot cooling. 2 cl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
INGOT-FORMING EQUIPMENT | 2007 |
|
RU2374032C2 |
MOLD OF MACHINE FOR CONTINUOUS CASTING OF BLANKS | 1997 |
|
RU2120347C1 |
METHOD FOR REPAIR OF MOLD OF CONTINUOUS CASTING MACHINE AND MOLD FOR ITS EMBODIMENT | 1996 |
|
RU2098222C1 |
METAL CONTINUOUS POURING CRYSTALLIZER | 1994 |
|
RU2030955C1 |
MOLD SLEEVE FOR CONTINUOUS STEEL CASTING | 2017 |
|
RU2678556C1 |
MOLD FOR CONTINUOUSLY CASTING METALS | 1996 |
|
RU2095189C1 |
COMBINED CRYSTALLIZER FOR CONTINUOUS INGOT CASTING | 1992 |
|
RU2015820C1 |
MOULD FOR CONTINUOUS CASTING OF METALS | 1996 |
|
RU2100134C1 |
MOULD FOR CONTINUOUS CASTING OF METALS | 1996 |
|
RU2100133C1 |
LINER HIGH-SPEED CONTINUOUS-CASTING CRYSTALLISER | 2007 |
|
RU2325969C1 |
Authors
Dates
1994-01-30—Published
1992-09-28—Filed