FIELD: metallurgy. SUBSTANCE: cupola bottom is made at an angle of 45-60 to the shaft axis, a hearth tuyere is inserted from the side of the shaft with extension of 0.9-1.1 of the furnace radius. EFFECT: reduced lining erosion and improved reliability. 4 dwg