FIELD: rubber-processing industry. SUBSTANCE: method comprises heat treating polymer comprising bonded maleic anhydride units with p-aminodiphenyl amine in organic solvent. Polymer is low weight (co)polymer based on diene monomers with average molecular weight from 600 to 2000, said (co)polymer containing grafted moleic anhydride units in amount from 10 to 30 wt %, at weight ratio of grafted maleic anhydride units to p-aminodiphenyl amine of 1:0.9- 1.9, respectively, at temperature from 20 to 90 C. Spatially hindered phenol is added to original reaction mixture. Method makes it possible to prepare polymeric antioxidant which protects natural rubbers and rubbers from thermooxidative and light aging. EFFECT: more efficient preparation method. 3 cl, 20 ex, 8 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STABILIZING EMULSION-POLYMERIZATION RUBBERS | 1996 |
|
RU2123015C1 |
METHOD OF STABILIZATION OF EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130031C1 |
METHOD OF PREPARING ANTIOXIDANT FOR EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130013C1 |
METHOD OF PREPARING EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130035C1 |
METHOD FOR PRODUCTION OF BUTADIENE-STYRENE(α-METHYL STYRENE) RUBBER BEING MODIFIED BY POLAR MONOMER | 1996 |
|
RU2115664C1 |
METHOD OF PRODUCING PHENYLENEDIAMINE ANTIOXIDANT FOR EMULSION-POLYMERISED RUBBER | 2007 |
|
RU2373184C2 |
METHOD OF SYNTHESIS BUTADIENESTYRENE RUBBER MODIFIED WITH POLAR MONOMER | 1995 |
|
RU2064925C1 |
METHOD OF PREPARING THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2113445C1 |
UNCOLORING STABILIZER FOR SYNTHETIC RUBBERS | 1996 |
|
RU2124532C1 |
POLYMERIC COMPOSITION | 1995 |
|
RU2064946C1 |
Authors
Dates
1999-05-10—Published
1996-12-25—Filed