FIELD: ferrous metallurgy technology. SUBSTANCE: samples are placing to elastic container at temperature about 80-100 C together with hardening material which volume must be equal to 1,2-1,3 of open porosity volume of samples. After hardening processing finishing samples are replaced down, cutting off, grinding and polishing. EFFECT: better sample preparing for structural analysis. 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MECHANICAL TREATMENT OF SINTER | 0 |
|
SU1696529A1 |
METHOD OF CHECK AND CONTROL OF QUALITY OF AGGLOMERATED CAKE | 1997 |
|
RU2111428C1 |
METHOD OF BREAKING AGGLOMERATION CAKE IN JAW CRUSHER | 0 |
|
SU1715869A1 |
METHOD OF AGGLOMERATION WITH RECYCLING OF EFFLUENT GASES | 1997 |
|
RU2119539C1 |
SINTER CAKE PRODUCTION METHOD | 0 |
|
SU1439138A1 |
MEHOD OF STABILIZING GRANULOMETRIC COMPOSITION OF SINTER | 0 |
|
SU1148884A1 |
AGGLOMERATE MANUFACTURE PROCESS | 2003 |
|
RU2248404C1 |
METHOD OF MANUFACTURING SINTER CAKE | 0 |
|
SU1308638A1 |
PROCESS FOR AGGLOMERATION OF PHOSPHATE ROCK | 0 |
|
SU1819850A1 |
METHOD OF DETERMINING STRUCTURE OF AGGLOMERATION SINTERING | 0 |
|
SU1344799A1 |
Authors
Dates
1994-04-15—Published
1990-12-29—Filed