FIELD: enrichment of useful minerals. SUBSTANCE: base and control flotation of origin material is carried out to produce foam and chamber product. Chamber product is additionally ground, then its control flotation to produce concentrate and tails is carried out. Said grinding is carried out within 1-30 min in uninterrupted regime. The process takes place in spring mill, minimal rotation rate of operated organ being 2.0-40 m/s, ratio solid and liquid products being 2.0: 1.0-5.0: 1.0. Foam product of base flotation is additionally ground. The process takes place in spring mill. Concentrate of control flotation is affected by additional grinding followed by selection. EFFECT: improves efficiency of the method. 5 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CONCENTRATING POTASSIUM CONTAINING ORE | 2007 |
|
RU2354457C1 |
SELECTIVE EXTRACTION METHOD OF COPPER MINERALS TO CONCENTRATES AT ENRICHMENT OF COPPER-ZINC PYRITE-CONTAINING ORES | 2009 |
|
RU2425720C1 |
METHOD FOR ENRICHMENT POLYMETALLIC ORES CONTAINING NICKEL, COPPER AND IRON SULFIDE MINERALS | 2015 |
|
RU2613687C1 |
METHOD FOR PRODUCING HIGH-QUALITY MAGNETITE CONCENTRATES | 2020 |
|
RU2754695C1 |
PROCESS OF DRESSING OF MINERAL STARTING MATERIALS CONTAINING PYROPHYLLITE ( VARIANTS ) | 2002 |
|
RU2222384C2 |
METHOD FOR DIRECT SELECTIVE FLOTATION OF LEAD-ZINC ORES | 2019 |
|
RU2713829C1 |
METHOD FOR ARRANGING PULP FOR FLOTATION OF MAGNETIC FRACTION FROM CONCENTRATES OF SULPHIDE COPPER-NICKEL ORES CONTAINING FERROMAGNETIC MINERALS OF IRON AND PRECIOUS METALS | 2008 |
|
RU2370316C1 |
METHOD OF DRESSING HIGH-SLIME POTASSIUM-BEARING ORES | 2011 |
|
RU2467803C2 |
METHOD OF CONCENTRATION OF COPPER-CONTAINING SLAGS | 1997 |
|
RU2130808C1 |
INTEGRATED APATITE-NEPHELINE ORE CONCENTRATION PROCESS | 1999 |
|
RU2152258C1 |
Authors
Dates
1994-05-15—Published
1991-11-25—Filed