FIELD: metallurgy. SUBSTANCE: method involves mixing lignin with mineral filler followed by calcination at 400-1200 C, coefficient of excess of air SiO2 being 0.5-0.9. Mentioned above filler contains α as a base, ratio lignin: filler being 1:0.25-2.0 as calculated for dry compound. Said filler additionally contains slag of cryolite production, its quantity being 40-80 mass %, quantity of material containing SiO2 20-60 as a base being 20-60 mass % . Slag of cryolite production is also used as CaO- and F - containing component of slag-forming mixture. EFFECT: improves protective and lubrication properties of desired product. 2 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING SLAG-MAKING MIXTURE | 0 |
|
SU1736672A1 |
SLAG-FORMING MIXTURE FOR CONTINUOUS CASTING OF STEEL | 2024 |
|
RU2825409C1 |
SLAG-FORMING MIXTURE FOR CONTINUOUS CASTING OF STEEL | 2024 |
|
RU2825408C1 |
SLAG FORMING MIXTURE FOR CONTINUOUS CASTING OF STEEL | 2018 |
|
RU2693706C1 |
SLAG-FORMING MIXTURE FOR CONTINUOUS STEEL POURING | 2014 |
|
RU2555277C1 |
SLAG-FORMING MIXTURE FOR STEEL CONTINUOUS CASTING | 2009 |
|
RU2378085C1 |
SLAG-FORMING MIXTURE FOR CONTINUOUS CASTING OF RAIL STEEL | 2010 |
|
RU2436653C1 |
SLAG-FORMING MIX FOR CONTINUOUS STEEL CASTING | 2010 |
|
RU2430808C1 |
SLAG-FORMING MIXTURE FOR CONTINUOUS CASTING RAIL STEEL | 2004 |
|
RU2260494C1 |
CHARGE FOR PRODUCTION OF MOLTEN BASE OF SLAG-FORMING MIX | 2009 |
|
RU2391178C1 |
Authors
Dates
1994-06-30—Published
1991-03-05—Filed