FIELD: construction. SUBSTANCE: injected into loessial slumping soil mass through injectors is loessial pulp with pressure gradually raised up to 3-10 atm. at rate of 3-5 cu.m/h for time needed to form hydrofrac in soil mass. Then, injection rate is reduced at least twice to discontinue further growth of hydrofrac value and wetting of mass zone round fracture. Cement-sand grout is injected at pressure of 3-10 atm. to compact soil in wetted zone up to achieve soil porosity of 38-40%. Loessial pulp contains clay particles in amount of 5-15%. Besides, injection of loessial pulp is carried out in opposite directions, e.g., by means of two-directional slotted injector. EFFECT: higher efficiency of soil compaction. 3 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR FORMATION OF GROUTING CURTAIN IN LOESSIAL SOIL | 1991 |
|
RU2015248C1 |
METHOD TO COMPACT COHESIVE DISPERSED SOILS | 2010 |
|
RU2425923C1 |
FOUNDATION PREPARATION METHOD | 2008 |
|
RU2380482C1 |
TILTED BUILDING STRAIGHTENING METHOD | 2004 |
|
RU2275473C1 |
METHOD OF COMPRESSING SOIL AND DEVICE FOR ITS IMPLEMENTATION | 2006 |
|
RU2324788C2 |
METHOD OF FLOATING PILE LOAD-BEARING CAPACITY INCREASE | 2004 |
|
RU2275470C1 |
PROCESS OF PREPARATION OF FOUNDATIONS | 1995 |
|
RU2122068C1 |
SLIDING SLOPE CONSOLIDATION METHOD | 2004 |
|
RU2275467C1 |
PROCESS OF CONSOLIDATION OF WATER-SATURATED GROUND IN FOUNDATIONS OF BUILDINGS AND STRUCTURES | 2002 |
|
RU2204650C1 |
METHOD TO COMPACT SOIL AND DEVICE FOR ITS REALISATION | 2012 |
|
RU2535564C2 |
Authors
Dates
1994-06-30—Published
1991-12-27—Filed