FIELD: refractory materials. SUBSTANCE: mortar has, wt.-%: refractory filler 55-75; aluminium 2-5; iron oxide 6-15, and temporary binder 17-25. Articles are glued and roasted at 1400-1450 C. Properties: limit of bending strength at 1200 C is 31-98 MPa, slag-resistance is 1.6-34.2%. EFFECT: enhanced quality of mortar. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY BINDING MORTAR | 0 |
|
SU1821460A1 |
REFRACTORY MORTAR | 0 |
|
SU1827374A1 |
MASS FOR ROASTING REFRACTORY ARTICLE FORMING | 1991 |
|
RU2021228C1 |
METHOD OF FABRICATING CLOSE-ROASTED CLINKER OF A HIGH-PURITY CARBONATE RAW MATERIAL | 1991 |
|
RU2068822C1 |
METHOD FOR GRAPHITE BEARING MASS PREPARATION | 1991 |
|
RU2016874C1 |
STOCK FOR MAKING REFRACTORY PRODUCTS | 0 |
|
SU1719361A1 |
SILICONIZING FILL FOR BURNING CARBIDE-SILICON ELECTRIC HEATERS | 1992 |
|
RU2039419C1 |
MORTAR FOR PASTING TOGETHER OF THE ALUMINA CERAMICS | 2004 |
|
RU2289553C2 |
REFRACTORY MORTAR | 2002 |
|
RU2228310C2 |
0 |
|
SU471338A1 |
Authors
Dates
1994-07-30—Published
1991-06-20—Filed