FIELD: metallurgy. SUBSTANCE: material has the following components, wt.-%: glass 8.1-13.2; molybdenum disulfide 1.0-3.5; aluminium 0.2-8.5; iron 0.1-3.2; tin 0.05-0.20, and copper - the rest. EFFECT: enhanced quality of antifriction material. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ANTIFRICTION MATERIAL BASED ON COPPER | 2014 |
|
RU2583976C1 |
METHOD OF PREPARING OF POWDER MATERIAL MADE ON COPPER-BASE WITH SILICON CARBIDE | 1991 |
|
RU2017852C1 |
COPPER POWDER-BASED ANTIFRICTION COMPOSITE | 2014 |
|
RU2576740C1 |
ANTIFRICTION COMPOSITION | 2022 |
|
RU2780264C1 |
COPPER-BASED POWDER-LIKE ANTI-FRICTION COMPOSITE MATERIAL | 2002 |
|
RU2223341C1 |
ANTI-FRICTION DISPERSION-HARDENED COMPOSITE MATERIAL | 1999 |
|
RU2203973C2 |
COPPER-BASED POWDER ANTIFRICTION COMPOSITE MATERIAL | 2009 |
|
RU2395602C1 |
COPPER-BASE POWDER MATERIAL | 0 |
|
SU1622414A1 |
IRON BASE POWDER ANTIFRICTION MATERIAL | 2003 |
|
RU2246377C1 |
ANTIFRICTION MATERIAL "ROMANIT", METHOD OF PREPARATION THEREOF, AND FRICTION UNIT MEMBER | 2001 |
|
RU2201431C2 |
Authors
Dates
1994-08-15—Published
1990-11-02—Filed