FIELD: manufacture of nonannealed building articles. SUBSTANCE: a mixture containing 1-3 wt % silicate lump and 97-99 wt % sand is prepared. The silicate lump and 30-50 wt % sand are "jointly comminuted, then mixed with the remainder of sand and flooded with water. The resulting mixture having a water to solid ratio of 0.1-0.12 is used to mold articles at a pressure of 10-20 MPa which are first steamed under atmospheric pressure at 80-90 C, a moisture content of 90-100% for 1-1.5 hr, then dried at 110-120 C for 2-3 hr. When the decorative shape of articles is desired, their surface is subjected to glazing by applying a low-temperature plasma. EFFECT: improved properties of the title products. 2 cl, 2 tbl, 5 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING UNBURNED BUILDING PRODUCTS | 2000 |
|
RU2168481C1 |
METHOD OF MANUFACTURING BUILDING PRODUCTS | 2012 |
|
RU2502697C2 |
PROCESS FOR MANUFACTURING FIRECLAYS | 1994 |
|
RU2082699C1 |
METHOD OF MANUFACTURE OF BUILDING ARTICLES | 1999 |
|
RU2165397C1 |
COMPOSITION AND PROCEDURE FOR FABRICATION OF NON-FIRED CHROMIUM-MAGNESITE HEAT RESISTANT CONCRETE | 2008 |
|
RU2377219C1 |
COMPOSITION AND PROCEDURE FOR FABRICATION OF NON-FIRED CHAMOTTE HEAT RESISTANT CONCRETE | 2008 |
|
RU2377217C1 |
METHOD OF PRODUCING UNFIRED REFRACTORIES | 0 |
|
SU1701693A1 |
COMPOSITION AND METHOD OF MAKING UNFIRED QUARTZITE HEAT-RESISTANT CONCRETE | 2008 |
|
RU2374202C1 |
COMPOSITION AND PROCEDURE FOR FABRICATION OF NON-FIRED DOLOMITE HEAT RESISTANT CONCRETE | 2008 |
|
RU2377220C1 |
COMPOSITION AND PROCEDURE FOR FABRICATION OF NON-FIRED MAGNESITE HEAT RESISTANT CONCRETE | 2008 |
|
RU2377218C1 |
Authors
Dates
1994-08-30—Published
1992-09-25—Filed