FIELD: technology of wear-resistant coating applying. SUBSTANCE: to enhance wear-resistance of workable tools and members at tempering temperature below 300 C nitrides of refractory metals of IV-VI groups of periodic law system are used for applying of wear-resistant coating in combination with thermal working. Wear-resistant films are applied by known method on the articles at the base temperature 400-800 C before hardening, and the following hardening (cooling) is carried out in the inert gaseous medium. EFFECT: enhanced wear-resistance of workable tools and members. 2 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CUTTING TOOLS HARDENING | 0 |
|
SU1765255A1 |
METHOD OF CUTTING TOOL HARDENING, MADE OF HIGH-SPEED STEEL | 0 |
|
SU1770448A1 |
STEEL PIECES HARDENING METHOD | 1992 |
|
RU2048606C1 |
PROCESS OF HARDENING OF HARD-ALLOY CUTTING TOOL | 1999 |
|
RU2167216C1 |
METHOD OF STRENGTHENING METAL-CUTTING TOOLS | 1993 |
|
RU2101382C1 |
METHOD OF WEAR-RESISTANT COATING FORMATION ON SURFACE OF ARTICLES MADE OF STRUCTURAL STEEL | 1998 |
|
RU2131480C1 |
METHOD FOR APPLYING INTERMITTENT WEAR-RESISTANT COATINGS | 0 |
|
SU1812238A1 |
METHOD OF ION-PLASMA TREATMENT OF STEEL AND HARD ALLOY PARTS | 2008 |
|
RU2370570C1 |
METHOD FOR HARDENING STEEL PRODUCTS | 1992 |
|
RU2009272C1 |
METHOD FOR COMPLEX ION-PLASMA TREATMENT OF METAL CUTTING TOOLS FROM HIGH-SPEED STEEL | 2024 |
|
RU2822379C1 |
Authors
Dates
1994-09-15—Published
1991-06-17—Filed