FIELD: metallurgy. SUBSTANCE: to the charge containing a nickel-containing material, pyrite as a sulfidizing agent, coke ar a reducing agent and as a fuel, a calcium-containing flux, a flux is shale as a calcium-containing flux, the ratio of the ingredients (wt %): 56-72 a nickel-containing material; 15-19 coke; 2.3-4.5 pyrite; 10.7-20.5 shale. EFFECT: improved processibility of the charge. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PREPARATION OF CHARGE TO MELTING FOR PRODUCTION OF NICKEL MATTE OUT OF OXIDISED NICKEL ORE | 2008 |
|
RU2389811C1 |
CHARGING MATERIAL FOR REDUCING SULPHIDING MELTING OF OXIDIZED NICKEL ORE | 2017 |
|
RU2657267C1 |
CHARGE FOR BLAST SMELTING OF OXIDIZED NICKEL-CONTAINING MATERIALS | 1993 |
|
RU2065504C1 |
METHOD FOR PRODUCING NICKEL MATTE | 2000 |
|
RU2184162C2 |
SULFIDIZING AGENT FOR REDUCTION SULFIDIZING CHARGE FOR MELTING OXIDIZED NICKEL ORES | 2001 |
|
RU2212461C2 |
METHOD OF NICKEL MATTE PRODUCTION | 2001 |
|
RU2187568C1 |
METHOD OF PRODUCING NICKEL MATTE | 2010 |
|
RU2441082C1 |
METHOD TO PRODUCE NICKEL MATTE | 2011 |
|
RU2455375C1 |
PROCESS OF REDUCTIVE-SULFIDIZING BLAST SMELTING OF OXIDIZED NICKEL ORES | 2001 |
|
RU2211252C2 |
0 |
|
SU488872A1 |
Authors
Dates
1994-09-30—Published
1990-02-05—Filed