FIELD: metallurgy.
SUBSTANCE: burden containing pelletised oxidised nickel-containing or and reducing fuel are loaded into shaft furnace. Then, reducing-sulphiding smelting is carried out using coke reduction agent as fuel. Note here that said coke is produced by carbonising the burden containing 5 to 100% of product, the yield of volatile substances making some 14-25%, obtained by delayed low-temperature carbonisation of heavy oil residues.
EFFECT: reduced fuel consumption higher smelting rate of nickel-containing stock, reduced nickel content in slug.
3 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF PRODUCING COPPER MATTE | 2010 | 
 | RU2441080C1 | 
| METHOD OF PYROMETALLURGICAL PROCESSING OF COPPER-CONTAINING MATERIALS | 2010 | 
 | RU2441081C1 | 
| METHOD OF PRODUCING MINERAL WOOL | 2010 | 
 | RU2439006C1 | 
| METHOD OF NICKEL MATTE PRODUCTION | 2001 | 
 | RU2187568C1 | 
| METHOD FOR PRODUCING NICKEL MATTE | 2000 | 
 | RU2184162C2 | 
| METHOD OF PRODUCING COKE | 2016 |  | RU2613051C1 | 
| METHOD TO PRODUCE NICKEL MATTE | 2011 | 
 | RU2455375C1 | 
| METHOD OF METALLURGICAL COKE PRODUCTION | 2013 | 
 | RU2553116C1 | 
| PULVERISED COAL FUEL FOR BLAST-FURNACE SMELTING | 2012 | 
 | RU2490316C1 | 
| 0 | 
 | SU254471A1 | 
Authors
Dates
2012-01-27—Published
2010-07-29—Filed