FIELD: manufacture of building materials. SUBSTANCE: 3.5-4.5 % by weight of bensoyl peroxide based on polyester resin is dissolved in acetone in the 1:1.6-1:2.5 ratio. The resulting solution is mixed together with polyester resin, and the resulting mixture is allowed to stand for 20-28 h. Thereafter, to the mixture a filling material is added under careful stirring. The obtained resin concrete material is placed into a mold treated with an antitacking agent. The mold is placed to a drying heated stove at 100-120 C for 30-60 min. The facing slab is released from the mold after cooling it. EFFECT: increased compression strength. 1 cl, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| DECORATING FACING PLATE PRODUCTION METHOD | 1991 | 
									
  | 
                RU2038341C1 | 
| PROCESS FOR MANUFACTURING FACING SLAB | 1991 | 
									
  | 
                RU2022945C1 | 
| POLYMER-CONCRETE MIXTURE FOR MAKING OF DECORATIVE FACING TILES | 1991 | 
									
  | 
                RU2026841C1 | 
| METHOD OF MAKING DECORATIVE ARTICLES | 1991 | 
									
  | 
                RU2022942C1 | 
| FACING SLAB MANUFACTURING PROCESS | 1991 | 
									
  | 
                RU2021114C1 | 
| METHOD OF MANUFACTURING FACING PLATE | 0 | 
									
  | 
                SU1761551A1 | 
| METHOD OF MAKING FACING TILES | 1991 | 
									
  | 
                RU2038216C1 | 
| FACING SLAB MANUFACTURING PROCESS | 1991 | 
									
  | 
                RU2021113C1 | 
| METHOD OF DECORATIVE-ARTISTIC ARTICLES PRODUCTION | 0 | 
									
  | 
                SU1763213A1 | 
| METHOD OF PRODUCING FACING TILES | 0 | 
									
  | 
                SU1502411A1 | 
Authors
Dates
1994-11-15—Published
1991-06-28—Filed