FIELD: building materials. SUBSTANCE: polymer-concrete mixture has, mas. p. : epoxide diane resin 20; polyethylenepolyamine 5-9; filler - waste of coal mining - burnt rocks or ash slag - 300-600; hardening agent on the basis of condensation product of phenol, formalin and ethylenediamine 3-15. Compression strength of tile made is 67-84 MPa, time of strengthening is 6-19 h. EFFECT: enhanced quality of mixture. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FACING SLAB MANUFACTURING PROCESS | 1991 |
|
RU2021113C1 |
PROCESS OF MANUFACTURING FACING SLAB | 1991 |
|
RU2022944C1 |
PROCESS FOR MANUFACTURING FACING SLAB | 1991 |
|
RU2022945C1 |
FACING SLAB MANUFACTURING PROCESS | 1991 |
|
RU2021114C1 |
DECORATING FACING PLATE PRODUCTION METHOD | 1991 |
|
RU2038341C1 |
METHOD OF MAKING FACING TILES | 1991 |
|
RU2038216C1 |
METHOD OF MAKING DECORATIVE ARTICLES | 1991 |
|
RU2022942C1 |
METHOD OF MANUFACTURING FACING PLATE | 0 |
|
SU1761551A1 |
COVERING PLATE MANUFACTURING METHOD | 1991 |
|
RU2021147C1 |
METHOD FOR MANUFACTURE OF ARTISTIC GLASSWARE | 0 |
|
SU1799737A1 |
Authors
Dates
1995-01-20—Published
1991-12-28—Filed