FIELD: metallurgy, machine engineering. SUBSTANCE: method involves addition of filtered off aqueous solution from the stage of semiproduct synthesis 4-amino-6-methoxypyrimidine at concentration 0.05-0.2% of composition to the working medium, wt.-%: resinoid products of oxidation and condensation of 4-amino-6-chloropyrimidine 25-30; 4-amino-6-methoxypyrimidine 2-3; NaCl 9-10, and water - the rest. Filtration is carried out at 3-5 C up to pH 9.0-9.5. Method is used for protection of carbonic, alloyed steel and alloy against corrosion lesion appearing under acid media action. EFFECT: improved method of protection. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROTECTION OF METALS | 1992 |
|
RU2061099C1 |
INHIBITOR OF ACID CORROSION | 1992 |
|
RU2064976C1 |
COMPOSITION FOR CHROME-PLATING OF STEELS AND PROCESS FOR PREPARING THEREOF | 1990 |
|
RU2020189C1 |
METHOD OF CORROSION INHIBITION AND COMPOSITION FOR METHOD EMBODIMENT | 2001 |
|
RU2198245C2 |
INHIBITOR FOR PROTECTION OF REACTION EQUIPMENT FROM CORROSION | 2014 |
|
RU2571243C1 |
CORROSION INHIBITOR | 1998 |
|
RU2160326C2 |
INHIBITOR FOR CORROSION PROTECTION OF REACTION EQUIPMENT | 2015 |
|
RU2588615C1 |
INHIBITOR OF CARBONIC ACID CORROSION FOR STEAM BOILERS OF LOW AND MEDIUM PRESSURE AMINAT PK-2 | 2012 |
|
RU2516176C2 |
WATER-SOLUBLE METAL CORROSION INHIBITOR | 2013 |
|
RU2528922C1 |
INHIBITING COMPOSITION FOR PROTECTION OF METALS FROM ACID CORROSION | 2015 |
|
RU2593569C1 |
Authors
Dates
1994-11-15—Published
1991-06-25—Filed