FIELD: baking industry. SUBSTANCE: method involves sand-blasting the internal surface of mold, heating it to 415-430 C, applying a coating of fluoroplastic material F-4MD and heat-treating the surface at the same temperature for 20-30 min. Coating is applied to a thickness of 10-20 microns. EFFECT: higher heat resistance of antiadhesive film at temperatures above 300 C. 1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR COVERING BY AUTOPHORESIS METHOD | 2005 |
|
RU2289601C1 |
METHOD FOR ANTIADHESION COATING APPLICATION ONTO BAKING TINS | 2011 |
|
RU2463790C1 |
ANTI-BURNING, ANTI-ADHESION AND WEAR-RESISTANT COAT | 2004 |
|
RU2256681C1 |
COMPOSITION FOR ANTIBURNING, ANTIADHESIVE, ANTICORROSION COATING BEING PRODUCED BY HETEROADAGULATION METHOD | 1994 |
|
RU2087506C1 |
COMPOSITION FOR PREPARING COVER BY AUTOPHORESIS METHOD | 2006 |
|
RU2298572C1 |
METHOD OF MICRO ARC OBTAINING OF COMPOSITE COATING ON ALUMINIUM AND ITS ALLOYS | 2011 |
|
RU2466218C1 |
METHOD OF PREPARING OF POLYIMIDE ANTIADHESION COATING | 1992 |
|
RU2021296C1 |
METHOD FOR COATING BAKING OF BREAD FORMS WITH ANTIADHESION COMPOSITION | 0 |
|
SU1750572A1 |
ANTIADHESION COATING | 2001 |
|
RU2198959C2 |
METHOD OF APPLICATION OF COAT ON METAL SURFACE, COMPOSITION OF PRIMER COAT AND COMPOSITION OF DECORATIVE COAT | 1999 |
|
RU2170286C1 |
Authors
Dates
1995-01-09—Published
1991-07-02—Filed