FIELD: shock-resistant compositions. SUBSTANCE: after heating the reaction mixture containing the following components (wt parts): 100 aminodecanic acid; 0.010.03 o-phthalatoethylene diamine copper; 0.04-0.07 stabilizer; 0.05-0.4 adipic acid to 260 ± 5 C and subsequent reduction of pressure to atmospheric 8-16 wt parts of N-butylbenzenesulfonamide per 100 wt perts of aminododecanic acid are added. EFFECT: improved properties of the shock-resistant composition. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF POLYAMIDE PLASTICIZED COMPOSITION PREPARING | 0 |
|
SU1819269A3 |
THERMOPLASTIC POLYMER MATERIAL | 1996 |
|
RU2115672C1 |
POLYMER PIEZOELECTRIC MATERIAL | 1993 |
|
RU2036182C1 |
METHOD OF BLOCK-COPOLYMER PREPARING | 1992 |
|
RU2036933C1 |
THERMAL PLASTIC COMPOSITION | 1995 |
|
RU2076121C1 |
POLYMER COMPOSITION | 1992 |
|
RU2028337C1 |
METHOD FOR PRODUCTION OF POLYAMIDE BY ANIONIC POLYMERIZATION OF CAPROLACTAM | 1992 |
|
RU2074866C1 |
PLASTICIZED POLYMERIC COMPOSITION | 1992 |
|
RU2036205C1 |
METHOD OF PRODUCING THE POLYHALOID ANION-EXCHANGE RESIN | 1995 |
|
RU2083604C1 |
THERMOPLASTIC POLYMER COMPOSITION | 1992 |
|
RU2057152C1 |
Authors
Dates
1995-01-09—Published
1992-01-30—Filed