FIELD: antifriction materials. SUBSTANCE: blanks were formed from material containing fluoroplastic and magnetic component by impregnation of porous coal-graphite base firstly with magnetite aqueous suspension containing 9-10 wt.-% ferrous oxide and then - with 45-55 wt.-% fluoroplastic aqueous suspension. As a result magnetic antifriction material is prepared containing, wt. -% : coal-graphite 69.5-87.4; magnetite 3.4-15.3; fluoroplastic 6-20. EFFECT: improved method of antifriction material preparing. 4 cl, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PREPARING OF STABLE LIQUID NONCRYSTALLIZING ALUMINIUM ALKOXIDES | 1991 |
|
RU2021248C1 |
| PROCESS FOR PREPARING CADMIUM COATINGS | 1990 |
|
RU2021392C1 |
| METHOD OF DIMETHYLIZINC PRODUCING | 1996 |
|
RU2117009C1 |
| METHOD OF REMOVING ALKYL COMPOUNDS OF GROUP II-VI INTRANSITION ELEMENTS FROM ALKYL HALIDE BY RECTIFICATION, AND RECTIFICATION COLUMN FOR CARRYING SAID METHOD INTO EFFECT | 1996 |
|
RU2111968C1 |
| BEE VENOM COLLECTOR | 1991 |
|
RU2032333C1 |
| REACTOR FOR STUDYING REACTION KINETICS | 0 |
|
SU1745330A2 |
| METHOD FOR DESTRUCTION OF LEWISITE | 1996 |
|
RU2106168C1 |
| METHOD OF COMPACTING AND PURIFYING AMORPHOUS ARSENIC | 1999 |
|
RU2170279C2 |
| DISTANCE MEASURING METHOD | 1992 |
|
RU2121699C1 |
| METHOD OF POLYCRYSTALLINE CADMIUM TELLURIDE BLOCK PRODUCTION | 0 |
|
SU1791425A1 |
Authors
Dates
1995-01-09—Published
1991-09-30—Filed