FIELD: polyethylene film-fiber cables. SUBSTANCE: mixture is prepared from cyclohexane of 5-25% of polyethylene from its mass and that of cyclohexane and 2% of water from cyclohexane mass. Mixture is molded at pressure higher than autogenous value and at temperature of 140-224 C into zone with lower temperature and pressure. EFFECT: facilitated procedure. 1 tbl