FIELD: chemistry of high-molecular compounds. SUBSTANCE: method for production of flexible and incombustible polyamide foams includes reaction of aromatic tetracarboxylic acid or its dianhydrate with aqueous solution of aliphatic alcohol when heating up to boiling with addition at room temperature of heterocyclic, aromatic and oliphatic diamine and heat-resistant cationic fluoro-containing surfactant with molecular mass of 625-670, taken from group specified in invention description in the amount of 4.0-10.0% of mass of reacting substances, drying of reaction products, their grinding and heat treatment. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SYNTHESIS OF ELASTIC AND FIRE-RESISTANT FOAM POLYIMIDES | 1990 |
|
SU1824885A1 |
METHOD OF SYNTHESIS OF ELASTIC AND FIRE-RESISTANT FOAM POLYIMIDES | 1990 |
|
SU1824886A1 |
COMPOSITION FOR PREPARING POLYIMIDE FOAM MATERIALS | 1993 |
|
RU2081134C1 |
METHOD FOR PREPARING THERMOPLASTIC POLYIMIDE | 1994 |
|
RU2094441C1 |
CRYSTALLISABLE FUSIBLE POLYETHERIMIDE COMPOSITE | 2020 |
|
RU2755476C1 |
METHOD OF PREPARING OF POLYAMIDOACID SOLUTION FOR FIBER FORMING | 1991 |
|
RU2034861C1 |
METHOD OF MANUFACTURING PREVAPORATION COMPOSITE POLYMER MEMBRANE | 1994 |
|
RU2094105C1 |
METHOD FOR OBTAINING MELT POLYIMIDE BINDER OF POLYMERIZATION TYPE | 2017 |
|
RU2666734C1 |
0 |
|
SU331561A1 | |
HIGH-STRENGTH HIGH-MODULUS THERMAL-, FIRE-RESISTANT POLYIMIDE THREAD AND METHOD FOR PRODUCTION THEREOF | 2017 |
|
RU2687417C1 |
Authors
Dates
1995-02-09—Published
1989-05-10—Filed