FIELD: chemical technology. SUBSTANCE: zirconium hydroxide is precipitated from zirconium nitrate solution containing 150-200 g/l zirconium and 350-430 g/l nitric acid with 20-25% ammonia solution taken at stoichiometric quantity. Intermediate exposition of hydroxide gel formed at pH 2.4-2.8 is 5-10 min. Then precipitate is filtered off, washed with water at 80-95 C and dried. EFFECT: improved method of zirconium hydroxide preparing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
INORGANIC SPHERIC GRANULATED HYDRATED ION-EXCHANGE MATERIAL AND METHOD FOR ITS PRODUCTION | 1992 |
|
RU2034645C1 |
METHOD FOR PRODUCTION OF PERLY PIGMENT | 1992 |
|
RU2057156C1 |
METHOD FOR PRODUCING RARE-EARTH ZIRCONATES | 2022 |
|
RU2801227C1 |
METHOD FOR RECOVERY RARE-EARTH ELEMENTS OF APATITE | 1991 |
|
RU2049727C1 |
METHOD FOR PRODUCING A GRANULATED INORGANIC SORBENT | 2020 |
|
RU2756163C1 |
METHOD OF PRODUCING ZIRCONIUM OXIDE HAVING TETRAGONAL MODIFICATION FOR PRODUCING CATALYSTS | 2008 |
|
RU2400429C2 |
METHOD OF PRODUCING NANOCRYSTALLINE POWDER OF METAL OXIDES | 2010 |
|
RU2425803C1 |
PROCESS FOR PREPARING TITANIUM HYDROXIDE | 1992 |
|
RU2049066C1 |
METHOD FOR PRODUCING CERAMIC COMPOSITES BASED ON LANTHANUM ORTHOPHOSPHATE | 2022 |
|
RU2791913C1 |
METHOD OF PREPARING OXIDE NUCLEAR FUEL | 1994 |
|
RU2069393C1 |
Authors
Dates
1995-03-27—Published
1991-07-09—Filed