FIELD: etching. SUBSTANCE: polyester backing is subjected for etching at 100-120 C for 0.5-2 min in 87-90% sulfuric acid with addition of 5-10% formaldehyde following by washing with hot water - 80 C, not lower. EFFECT: increased adhesion of chemical coating to the backing. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF CHEMICAL ETCHING BACKING MADE OF TRIACETYLCELLULOSE BEFORE CHEMICAL METALLIZATION | 1991 |
|
RU2039848C1 |
| METHOD FOR MANUFACTURING OF PRINTED CIRCUITS | 1994 |
|
RU2081519C1 |
| METHOD FOR PRODUCING LOCAL COPPER COATINGS ON INSULATORS | 0 |
|
SU1067081A1 |
| SOLTUION FOR CHEMICAL COPPER PLATING | 0 |
|
SU983150A1 |
| METHOD OF CHEMICAL NICKEL PLATING OF GLASS | 1999 |
|
RU2167113C2 |
| PROCESS OF MANUFACTURE OF TWO-SIDE PRINTED CIRCUIT BOARDS FROM GLASS CLOTH- BASED LAMINATE | 1992 |
|
RU2040129C1 |
| METHOD FOR TREATMENT OF DIELECTRIC BEFORE CHEMICAL COPPER-PLATING | 0 |
|
SU1763434A1 |
| METHOD FOR NON-PALLADIUM ACTIVATION OF PLASTIC SURFACE | 2014 |
|
RU2588918C1 |
| METHOD FOR METALLIZATION OF CERAMIC PRODUCTS | 2021 |
|
RU2777312C1 |
| FLUOROPLASTIC SUBSTRATE METALLIZATION DEPOSITION METHOD | 1991 |
|
RU2020777C1 |
Authors
Dates
1995-03-27—Published
1990-03-16—Filed