FIELD: manufacture of building materials. SUBSTANCE: the polymeric concrete mix comprises, as an amine hardener, a mixture of polyoxypropylene amine with a molecular weight of 480-550 with dicyanoethyldiethylene triamine in a 1-3:1 ratio or a mixture of polyethylene amine with a molecular weight of 180-220 with dicyanoethyldiethylene triamine in a (- .33-1): ratio, the ratio of the components being as follows (wt %): 23.5-30.3 epoxydiane resin; 30.3-35.5 trig chloropolyol resin; 11.6-12.2 said amine hardener; 27.2-29.6 quartz sand. The resulting polymeric concrete has Grecelli attrition up to 0,003 g/cm2, a water absorption of up 0.18 % for 24 hours and a deactivation coefficient of up to 0.2. EFFECT: improved properties of the building materials. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERIC FLOORING COMPOSITION | 1995 |
|
RU2125582C1 |
POLYMER-CONCRETE MIX | 1995 |
|
RU2107669C1 |
POLYMER-CONCRETE MIXTURE | 1987 |
|
SU1517299A1 |
POLYMER-CONCRETE MIX POLYQUARTZITE | 2013 |
|
RU2537426C1 |
BINDER FOR APPLYING THE COATINGS | 0 |
|
SU1502518A1 |
POLYMER COMPOSITION FOR FRAMING IMPREGNATION | 2019 |
|
RU2717596C1 |
ADHESIVE COMPOSITION | 0 |
|
SU1806158A3 |
COATING COMPOSITION FOR CONCRETE SURFACE | 2003 |
|
RU2237695C1 |
EPOXY COMPOSITION | 2023 |
|
RU2807757C1 |
EPOXIDE COMPOSITION | 2000 |
|
RU2186077C2 |
Authors
Dates
1995-04-10—Published
1992-07-09—Filed