FIELD: optics. SUBSTANCE: composition includes, parts by mass: epoxy compound 100; bismuth oxychloride 1.0-3.5; antimony trioxide 6.0-2.8. EFFECT: increased sensitivity to IR laser radiation. 1 tbl