FIELD: fuel industry. SUBSTANCE: method involves addition of hardener to the liquid fuel - low-pressure polyethylene at concentration 8-14 mas. p. per 100 mas. p. mixture following by heating of latter and cooling. EFFECT: improved method of fuel preparing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARATION OF SOLIDIFIED HYDROCARBON FUEL TO USE AND PLANT FOR ITS REALIZATION | 1990 |
|
RU2289064C2 |
METHOD OF FABRICATING COAL BRIQUETS | 1994 |
|
RU2078794C1 |
COMPOSITION FOR PRODUCTION OF SOLID-FUEL PRODUCTS | 2015 |
|
RU2577851C1 |
METHOD OF FABRICATING FUEL BRIQUETTES | 1998 |
|
RU2125083C1 |
METHOD AND INSTALLATION FOR PREPARING AND BURNING SOLIDIFIED LIQUID HYDROCARBON FUELS | 0 |
|
SU1799903A1 |
COMPOSITE FUEL | 2018 |
|
RU2664330C1 |
MOTOR FUEL | 1994 |
|
RU2054452C1 |
MOTOR FUEL | 1994 |
|
RU2054453C1 |
FUEL BRIQUETTE AND FUEL BRIQUETTE PRODUCTION METHOD | 1994 |
|
RU2068442C1 |
METHOD OF PRODUCTION OF FUEL BRIQUETTES | 2004 |
|
RU2278891C1 |
Authors
Dates
1995-05-20—Published
1994-01-12—Filed