FIELD: radio electronics. SUBSTANCE: ceramic material mixture containing solid solution meeting common formula (Ba0,9Sr0,1)(Nd0,6Bi0,2La0,2)2Ti4O12 is added with glass forming additive of variable content xB2O3·ySiO2, where X=0.05-0.90; Y=0.10-0.95 in the amount of 1.0-2.0 per cent by mass. EFFECT: reduced sintering temperature of material up to 1060-1160 C and annealing temperature to 1060-1120 C with keeping dielectric permittivity value ε ~ 100 and capacitance C = 0,04 μF,. 3 tbl