FIELD: chemistry. SUBSTANCE: this process prescribes admixing in water phenol, formaldehyde, water-soluble furan compounds (10 to 20 percent by mass) in presence of catalyst and emulsifier, washing and filtering thus prepared polymer suspension, thermally solidifying resultant polymer stock by heating it at temperature of 270 to 280 C at temperature building-up rate of 10 to 15 C/h, carbonizing end product, and finally activating it. EFFECT: more advanced technique. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF SPHERICAL CARBON ADSORBENT | 1982 |
|
RU2073642C1 |
METHOD OF PRODUCING CARBON FIBROUS ADSORBENT | 1992 |
|
RU2049168C1 |
METHOD FOR PRODUCTION OF ACTIVATED CARBON | 1993 |
|
RU2057067C1 |
METHOD OF CARBON SORBENT PREPARING | 1993 |
|
RU2021010C1 |
METHOD OF PREPARING OF SPHERIC CARBON ADSORBENT | 1993 |
|
RU2026813C1 |
METHOD OF ACTIVATED CARBON PRODUCING | 1993 |
|
RU2023663C1 |
METHOD OF PRODUCTION OF GLOBULAR CARBON ADSORBENT | 2003 |
|
RU2257343C2 |
METHOD OF MANUFACTURING SPHERICAL CARBONACEOUS ADSORBENT | 2006 |
|
RU2301701C1 |
METHOD FOR PRODUCTION OF CRUSHED ACTIVATED COAL | 1997 |
|
RU2105714C1 |
METHOD OF CHARCOAL PREPARING | 1993 |
|
RU2031837C1 |
Authors
Dates
1995-05-27—Published
1993-02-04—Filed