FIELD: building materials production. SUBSTANCE: proposed binder contains (mass % ): clay 15-25, cement 25-40, base ash the rest. Compressive strength thus prepared binder at age of 28 days is 35.4-44.2 MPa. EFFECT: improves quality of binder. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDER | 1998 |
|
RU2155170C2 |
METHOD FOR PRODUCTION OF CEMENT AND RAW MEAL FOR MANUFACTURING CEMENT CLINKER | 1998 |
|
RU2138457C1 |
CRUDE MIXTURE FOR MAKING ASH-SLAG CONCRETE | 2011 |
|
RU2471745C2 |
CRUDE MIXTURE FOR MAKING ASH-SLAG CONCRETE | 2011 |
|
RU2479532C2 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF ASH-AND-SLAG CONCRETE | 2013 |
|
RU2553817C2 |
RAW MIXTURE FOR MAKING ASH AND ALKALI CONCRETE | 2013 |
|
RU2553818C2 |
COMPOSITION FOR ARRANGEMENT OF LOWER LAYER OF ROAD SURFACE BASE | 2011 |
|
RU2468139C2 |
ACTIVE MINERAL ADDITIVE FOR CEMENT AND METHOD FOR PREPARATION THEREOF | 2015 |
|
RU2581437C1 |
BINDER | 2011 |
|
RU2471734C2 |
METHOD OF PRODUCING ACID-RESISTANT CONCRETE | 2011 |
|
RU2470900C1 |
Authors
Dates
1995-05-27—Published
1991-07-25—Filed