FIELD: chemistry of polymers. SUBSTANCE: method of butadiene-styrene latex preparing involves two-stage polymerization of butadiene with styrene. Ratio of comonomers at the first and second stages is 1:(4.8-4.9). Mass ratio of butadiene and styrene at the first stage is 1:(5-7), and the second one is (3.0-3.3): 1, respectively. Method is realized in the presence of emulsifying agents, electrolyte and molecular mass regulator which is added at both the first and the second stages of process. Regulator concentration at the first stage is 0.19-1.11 wt.-% (as comonomer level at the first stage). Also, styrene can be added at the first stage at the level equal comonomer quantity used at the first stage. EFFECT: increased stability of reaction mass and latex prepared, increased output of process, enhanced physical-mechanical properties of films made of this latex. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR PREPARING BUTADIENE-STYRENE LATEX | 1994 |
|
RU2076874C1 |
ACRYLONITRILE/BUTADIENE/STYRENE COPOLYMER PRODUCTION PROCESS | 1999 |
|
RU2160286C1 |
METHOD OF MANUFACTURING POLYSTYRENE LATEX | 1995 |
|
RU2092496C1 |
METHOD OF PRODUCING BUTADIENE-STYRENE LATEX | 0 |
|
SU1183506A1 |
METHOD OF AUTOMATICALLY CONTROLLING PROCESS OF HYDROCARBON EMULSION PREPARATION IN BUTADIENE-STYRENE LATEX PRODUCTION | 1994 |
|
RU2083593C1 |
CARBOXYLATE LATEX THICKENING AGENT | 1994 |
|
RU2088610C1 |
METHOD OF PREPARING COPOLYMER LATEXES FOR ANTISTATIC COATINGS | 1998 |
|
RU2128671C1 |
RUBBER PRODUCTION PROCESS | 2001 |
|
RU2179173C1 |
METHOD OF BUTADIENE-(METHYL)STYRENE RUBBERS PRODUCING BY EMULSION POLYMERIZATION | 2015 |
|
RU2615748C1 |
METHOD OF PREPARING VINYLIDENE FLUORIDE- TETRAFLUOROETHYLENE COPOLYMERS | 1998 |
|
RU2139891C1 |
Authors
Dates
1995-05-27—Published
1992-05-26—Filed