FIELD: glueing materials. SUBSTANCE: glue composition has, % (as dry matter): latex of copolymer of butadiene with acrylonitrile and methacrylic acid at acrylonitrile link content 35-50 wt.-% 35-50; chalk 5-15; kaolin or talc 5-15; froth breaker 0.1-0.5; copolymer of acrylonitrile with methacrylic acid saponified with alkali, ammonia or triethanolamine at acrylonitrile link content 40 wt.-% 1.5-10.0, and water - the rest. Composition can contain additionally (% ) carboxymethylcellulose 1-6; surface-active substance 0.05-5.0, and zinc oxide 0.1-0.5. Glue properties: glueing strength at exfoliation is 2.7-3.2 kgf/cm. Glue is used for polychlorovinyl film glueing. EFFECT: enhanced quality of glue. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING AQUEOUS DISPERSIVE ADHESIVE | 1997 |
|
RU2132860C1 |
GLUEING COMPOSITION | 0 |
|
SU1766936A1 |
GLUE COMPOSITION | 0 |
|
SU1609805A1 |
ADHESIVE COMPOSITION | 1999 |
|
RU2160754C2 |
METHOD FOR PRODUCING CARBOXYLATED LATEX, CARBOXYLATED LATEX AND GLUE COMPOSITION ON ITS BASIS | 2017 |
|
RU2669837C1 |
GLUE FOR CIVIL ENGINEERING WORK | 1999 |
|
RU2164237C1 |
AQUEOUS DISPERSED PAINT | 1998 |
|
RU2124539C1 |
GLUEING COMPOSITION | 1993 |
|
RU2069225C1 |
AQUEOUS DISPERSIVE ADHESIVE COMPOSITION | 1998 |
|
RU2159263C2 |
GLUE | 0 |
|
SU729226A1 |
Authors
Dates
1995-06-09—Published
1992-08-05—Filed