FIELD: leather industry. SUBSTANCE: leather fabric is hydrophobized and greased simultaneously by the following manner. To 100 mas. p. p. of product obtained by fat rendering and collagen-containing waste from shreds and ends 1-6.5 mas. p. of acid and 3.5-65 mas. p. p. of poly(alkoxy)silsesquioxane are added. Obtained preparation at amount 1-7% of semifinished product mass is applied on its surface and subjected for vibrotreatment for 2-4 min at frequency 1-10 Hz. EFFECT: improved ecology, highly efficient production. 2 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DRESSING SKIN TISSUE | 1998 |
|
RU2135594C1 |
METHOD FOR PROCESSING OF LEATHER FABRIC | 1992 |
|
RU2036974C1 |
METHOD FOR DECORATING OF LEATHER AND FUR HALF-FINISHED PRODUCT | 1991 |
|
RU2036973C1 |
METHOD OF DRYING LEATHER AND FUR SEMIPRODUCT | 1991 |
|
RU2031951C1 |
METHOD OF PROCESSING SHEEPSKINS | 1995 |
|
RU2126839C1 |
PROCESS FOR COMBINED TUNING AND GREASE LIQUORING FUR SKINS | 0 |
|
SU941425A1 |
CRUDE FUR TREATMENT PROCESS | 2003 |
|
RU2225447C1 |
METHOD FOR SHEEPSKIN TREATMENT | 0 |
|
SU1730163A1 |
LIPOSOMAL COMPOSITION FOR TREATING LEATHER AND FUR SEMIFINISHED PRODUCT AND TREATMENT PROCESSES | 2003 |
|
RU2228361C1 |
CORIUM OF GENUINE LEATHER AND FUR SEMIFINISHED PRODUCT AND METHODS FOR MANUFACTURE THEREOF | 2002 |
|
RU2206620C1 |
Authors
Dates
1999-08-27—Published
1998-11-17—Filed