FIELD: metal protection against corrosion. SUBSTANCE: composition has, wt. -% polyvinyl chloride 55.6-66.0; low-pressure polyethylene 2-4; epoxy diane oligomer 6.6-9.5; dioctylphthalate 23-27; dicyandiamide 0.6-0.9; chrome oxide 1.8-3.0. Polyethylene is added to the mixer with polyvinyl chloride, pigment paste and epoxy diane oligomer, stirred at 100 C for 1 h and then at 25 C for 0.5 h up to homogeneous mixture formation. Coating is dried at 210 ± 2 C for 9-10 min. Properties: wear resistance is 7000-7250 double moves, adhesion strength is 770 H/m. EFFECT: enhanced quality of composition. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
POWDERY POLYMERIC COMPOSITION | 1990 |
|
RU2016009C1 |
METHOD OF POWDERY DYE PREPARING | 1991 |
|
RU2028345C1 |
POWDER COMPOSITION FOR PROTECTIVE COATING | 0 |
|
SU1836401A3 |
PLASTISOL BASED ON POLYVINYLCHLORIDE OR VINYL CHLORIDE/VINYL ACETATE COPOLYMER | 2002 |
|
RU2214438C1 |
PLASTISOL | 1998 |
|
RU2149166C1 |
POLYMER COMPOSITION | 2004 |
|
RU2266308C1 |
ANTI-CORROSION COMPOSITION | 2009 |
|
RU2405012C1 |
EPOXIDE-PERCHLOROVINYL COMPOSITION FOR PREPARING SELF-HEALING PAINT COATINGS | 2017 |
|
RU2673852C1 |
PLASTISOL COMPOSITION FOR SEALING AND DEPOSITING COATINGS | 2008 |
|
RU2382805C1 |
PRIMER COMPOSITION | 2011 |
|
RU2471841C1 |
Authors
Dates
1995-06-19—Published
1991-07-02—Filed