FIELD: electrical engineering. SUBSTANCE: aluminium alloy blank is coated with layer of contact nickel composed of nickel chlorine dissolved in acidic medium with addition of potassium fluoride, this procedure being followed by electric deposition of nickel at reversing current with anode pulse length of 0.1-0.3 s and anode- to-cathode pulse length ratio of 1:30 1:50 up to nickel layer thickness of 18-20 mcm. Copper plating is made at pulse current of 0.1-0.3 s length superposed on d.c. current until layer thickness of 12-15 mcm is attained. EFFECT: facilitated procedure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF APPLYING ELECTROCONDUCTIVE PROTECTIVE COATING ON ALUMINIUM ALLOYS | 2023 |
|
RU2817277C1 |
METHOD OF MANUFACTURE OF CONTACT CLAMPS FOR LINE ACCESSORIES | 0 |
|
SU1669019A1 |
METHOD OF MAKING AN ELECTRODE FROM REINFORCED LEAD DIOXIDE | 2019 |
|
RU2691967C1 |
FABRICATION OF IC CASE | 2013 |
|
RU2561240C2 |
METHOD FOR APPLICATION OF NICKEL COATINGS TO ALUMINUM ALLOYS | 2017 |
|
RU2661695C1 |
METHOD OF SURFACE PREPARATION OF STAINLESS STEEL ITEMS PRIOR TO GALVANIC COPPERPLATING | 2013 |
|
RU2549037C2 |
METHOD FOR PRODUCTION OF COMPOSITE METAL-CERAMIC COATING AT VALVE METALS AND THEIR ALLOYS | 2013 |
|
RU2543659C1 |
METHOD FOR PRODUCING METAL COATINGS ON ALUMINIUM | 0 |
|
SU1032047A1 |
METHOD FOR MAKING HOLLOW PARTS WITH OUTER ENVELOPE BY ELECTROPLATING | 0 |
|
SU1657543A1 |
PROCESS OF DEPOSITION OF METAL COATS ON ARTICLES MADE OF MAGNESIUM AND ITS ALLOYS | 1999 |
|
RU2150534C1 |
Authors
Dates
1995-06-19—Published
1992-12-24—Filed