FIELD: metallurgy. SUBSTANCE: lower part of nozzle is made in each sector when the sector is made. Lack of ring seam around the nozzle decreases consumption of electrodes for making disk (tip) of the lance and decreases possibility of burning out the lance tip. EFFECT: decreased amount of non-ferrous metal for making lance tip, and simplified manufacturing. 2 dwg
Title | Year | Author | Number |
---|---|---|---|
TIP OF OXYGEN-CONVERTER LANCE | 1998 |
|
RU2115745C1 |
TUYERE FOR BLOWING METAL IN CONVERTER | 0 |
|
SU1315480A1 |
TUYERE FOR BLAST OF METAL | 2009 |
|
RU2398026C1 |
METHOD OF MAKING WELDED STRAIGHT-SEAM TUBES | 1993 |
|
RU2040988C1 |
METHOD FOR MANUFACTURE OF WELDED TUBES WITH LONGITUDINAL SEAM | 1993 |
|
RU2049570C1 |
PROBE FOR MEASUREMENT OF LIQUID METAL PARAMETERS | 0 |
|
SU1772169A1 |
TUYERE FOR BLOWING MELT METAL | 2000 |
|
RU2181384C1 |
BLAST FURNACE TUYERE | 1999 |
|
RU2167204C1 |
LANCE FOR METAL BLOW IN CONVERTER | 0 |
|
SU1768648A1 |
METHOD AND OXYGEN LANCE FOR METALS SMELT BLOWING | 1995 |
|
RU2068001C1 |
Authors
Dates
1995-07-09—Published
1992-04-13—Filed