FIELD: oil production. SUBSTANCE: protective coating contains (mass): epoxy diane oligomer 15-25; furfural-acetone monomer 10-15; coal tar 5-10; mixture of product of reamination of 2-dimetylaminomethyl phenol by ethylene diamine and 2-aminphenol-4-sulfoacid at their mass ratio 1:(0.2-0.35) which is used as hardener 10-12; product prepared by mixing suspension of polymethylmethacrylate and benzoyl peroxide at ratio 1:(0.01-0.015) which is used as filler 20-40; and organic solvent. Coating is dried at 80-100 C within 1.5-4.0 h. EFFECT: improves efficiency of the method. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERIC COMPOSITION | 1992 |
|
RU2068426C1 |
PAINT COMPOSITION | 1986 |
|
RU1389195C |
METHOD OF SYNTHESIS OF HARDENER FOR EPOXY-DIANE RESINS | 0 |
|
SU1754709A1 |
CURING AGENT FOR EPOXY RESINS AND METHOD FOR ITS PRODUCTION | 1991 |
|
RU2028320C1 |
COMPOSITION FOR BONDING AND APPLYING COATINGS | 0 |
|
SU1775453A1 |
EPOXY PUTTY | 1992 |
|
RU2100394C1 |
COMPOSITION FOR WELL KILLING AND WELL COMPLETION | 1992 |
|
RU2092516C1 |
ENAMEL FOR DEPOSITING ANTICORROSION FIREPROOF BIORESISTANT COATING | 2008 |
|
RU2401854C2 |
ANTICORROSION PROTECTIVE POLYMERIC COATING | 2002 |
|
RU2216561C1 |
METHOD FOR SELECTIVE SHUTOFF INFLOW OF MINERALIZED FORMATION WATER IN WELLS | 1992 |
|
RU2069738C1 |
Authors
Dates
1995-09-10—Published
1992-06-16—Filed