FIELD: as protective corrosion resistant coatings. SUBSTANCE: polymeric composition comprises (wt%): 16-22 product resulting from grinding carboxymethyl cellulose containing 28-34% carboxy groups as filler and methaphenylene diamine in 1: 0.125-0.25 ratio; 43-48 furfuroacetone monomer; 20-28 epoxy diane oligomer; 10-13 polyethylene polyamine. Polymeric composition based coatings have insignificant shrinkage and increased compression strength with immersion rates of 4-20 mm/min. EFFECT: improved properties of the polymeric composition.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF PROTECTIVE COATING | 1992 |
|
RU2043376C1 |
EPOXY BINDER FOR COMPOSITE MATERIALS | 2021 |
|
RU2788335C1 |
0 |
|
SU1567550A1 | |
METHOD OF WELLS CASING AND CEMENTING | 1992 |
|
RU2068489C1 |
POLYMERIC BINDER | 0 |
|
SU1509378A1 |
COMPOUND FOR CONSOLIDATION OF BOTTOM-HOLE ZONE OF BED | 1997 |
|
RU2138616C1 |
BINDER FOR CARBON-CONTAINING REFRACTORIES | 0 |
|
SU1491853A1 |
COMPOSITION OF INHIBITOR OF GAS PIPELINE CORROSION | 1991 |
|
RU2023754C1 |
POLYMER COMPOSITION | 2019 |
|
RU2730311C1 |
COMPOSITION FOR WELL KILLING AND WELL COMPLETION | 1992 |
|
RU2092516C1 |
Authors
Dates
1996-10-27—Published
1992-08-24—Filed