FIELD: instrument making. SUBSTANCE: ceramic powder is heated at 120-140 C for 2-4 h and cooled up to 80-90 C. Then surface-active substance is added at concentration 0.3-1 wt.-% and binding and casting slip is carried out at 90-95 C under pressure 5-6 atm. Binder is calcined out at 100-110 C. Positive effect: Tc= 90-92K 90-92 K, ΔTc=2K 2 K, Jk= 50-150 A/cm3. Material is used for making devices using superconductivity. EFFECT: enhanced quality of material.
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR MAKING OF REFRACTORY CRUCIBLE AND SUPPORT | 1992 |
|
RU2028994C1 |
CHARGE FOR MAKING OF CERAMIC ARTICLES WITH COMPLEX CONFIGURATION | 1991 |
|
RU2021229C1 |
THERMOPLASTIC BINDER FOR FORMING CERAMIC PRODUCTS BY HOT INJECTION MOULDING | 0 |
|
SU1024438A1 |
METHOD OF PREPARING OF RARE-EARTH METALS YTTRIUM AND SCANDIUM | 1992 |
|
RU2013460C1 |
PROCESS OF MANUFACTURE OF LAYERS OF SILICON OXIDE | 1992 |
|
RU2013819C1 |
METHOD OF MANUFACTURING REINFORCED CERAMIC ARTICLE | 2001 |
|
RU2253566C2 |
PRODUCTION OF CERAMIC SLURRY | 2013 |
|
RU2531960C1 |
METHOD OF MAKING CERAMIC ARTICLES | 0 |
|
SU865859A1 |
METHOD OF THIOUREA ISOLATION | 1992 |
|
RU2027705C1 |
SOLID COMPOSITION FOR STORAGE AND TRANSPORT OF NATURAL GASES | 1995 |
|
RU2083488C1 |
Authors
Dates
1995-09-27—Published
1992-08-14—Filed