FIELD: chemical technology. SUBSTANCE: amorphous boron is mixed preliminary with isotactic polypropylene, pressed as blanks, chips were obtained by sharpening and crushed its up to powder state with dispersity 1 mm in ball mixer. Then polyethylene is added to crushed powder, mixed and extruded. Process is carried out at amorphous boron content 50-75 wt.-% per 100 wt.-% of its mixture with polypropylene. Product is used for biological protection against neutron radiation. EFFECT: improved method of composition preparing. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING HIGH-FILLED BORON-CONTAINING COMPOSITION | 2001 |
|
RU2197507C2 |
PROCESS OF PREPARATION OF BORON-CARRYING COMPOSITION | 2000 |
|
RU2196788C2 |
METHOD OF PREPARING POLYMERIC COMPOSITION | 1997 |
|
RU2124028C1 |
METHOD OF PREPARING GRAPHITE CONTAINING COMPOSITION | 1996 |
|
RU2103286C1 |
METHOD OF PREPARATION OF THE HIGHLY FILLED GRAPHITE- BEARING COMPOUND | 2002 |
|
RU2217448C2 |
POLYMER-BASED RADIATION-PROOF MATERIAL WITH HIGH RESISTANCE TO X-RAY AND NEUTRON RADIATION | 2014 |
|
RU2561989C1 |
METHOD OF PREPARING GRAPHITE-CONTAINING COMPOSITION | 1999 |
|
RU2162095C2 |
METHOD OF PREPARING GRAPHITE-CONTAINING COMPOSITIONS | 2000 |
|
RU2160290C1 |
BORON CONTAINING COMPOSITION | 1995 |
|
RU2096431C1 |
GRAPHITE-CONTAINING COMPOSITION PREPARATION METHOD | 2004 |
|
RU2272050C2 |
Authors
Dates
1995-12-20—Published
1992-12-24—Filed